EN 10025-2 : 2004 Technical delivery conditions for non-alloy structural steels
- S235JR Steel Grade, Mechanical Properties, Chem
- S235J0 Steel Grade, Mechanical Properties, Chem
- S235J2 Steel Grade, Mechanical Properties, Chem
- S275JR Steel Grade, Mechanical Properties, Chem
- S275J0 Steel Grade, Mechanical Properties, Chem
- S275J2 Steel Grade, Mechanical Properties, Chem
- S355JR Steel Grade, Mechanical Properties, Chem
- S355J0 Steel Grade, Mechanical Properties, Chem
- S355J2 Steel Grade, Mechanical Properties, Chem
- S355K2 Steel Grade, Mechanical Properties, Chem
- S450J0 Steel Grade, Mechanical Properties, Chem
- E295 Steel Grade, Mechanical Properties, Chemic
- E335 Steel Grade, Mechanical Properties, Chemic
- E360 Steel Grade, Mechanical Properties, Chemic
-
EN 10025-3:2004 - Technical delivery conditions for normalized/normalized rolled weldable fine grain structural steels
-
EN 10025-4:2004 - Technical delivery conditions for thermomechanical rolled weldable fine grain structural steels
-
EN 10025-5:2004 - Technical delivery conditions for structural steels with improved atmospheric corrosion resistance
-
EN 10025-6:2004 - Technical delivery conditions for flat products of high yield strength structural steels in the quenched and tempered condition
S235J2 Steel Grade, Mechanical Properties, Chemical Composition, Grade Equivalent
Standard: EN 10025-2:2004, European standard for hot-rolled structural steel. Part 2 - Technical delivery conditions for non-alloy structural steels.
Steel grade: S235J2 ;
Number: 1.0117;
Weldability: This steel grade is generally suitable to welding.
The table below show the mechanical properties of grade S235J2
Minimum yield strength Reh MPa |
Tensile strength Rm MPa |
Minimum elongation - A Lo = 5,65 * √So (%) |
Notch impact test |
|||||||||||
Steel grade | Nominal thickness mm |
Nominal thickness mm |
Nominal thickness mm |
Temperature |
Min. absorbed energy |
|||||||||
≤16 |
>16 ≤40 |
>40 ≤63 |
>63 ≤80 |
>80 ≤100 |
>100 ≤125 |
>3 ≤100 |
>100 ≤125 |
>3 ≤40 |
>40 ≤63 |
>63 ≤100 |
>100 ≤125 |
°C |
J |
|
S235J2 |
235 |
225 |
215 |
195 |
360-510 |
350-500 |
26 |
25 |
24 |
22 |
-20 |
27 |
The table below show the chemical composition of grade S235J2
Ladle analysis |
|||||||||||||
Steel grade | C max. % |
Mn max. % |
Si max. % |
P max. % |
S max. % |
N max. % |
Cu max. % |
Other max. % |
CEV max. % |
||||
Nominal thickness mm |
Nominal thickness mm |
||||||||||||
≤16 |
>16 ≤40 |
>40 |
≤30 |
>30 ≤40 |
>40 ≤125 |
||||||||
S235J0 | 0,17 |
0,17 |
0,17 |
1,40 |
- |
0,030 |
0,030 |
- |
0,55 |
- |
0,35 |
0,35 |
0,38 |
S235J2 Steel Grade Equivalent Table
USA |
England BS |
European old EN |
China GB |
Russia GOST |
A36 |
40EE |
Fe360D2 S235J2G4 |
Q235D |
17G1S |