EN 10025-5:2004 - Technical delivery conditions for structural steels with improved atmospheric corrosion resistance

EN 10025-5:2004 - European standard for hot-rolled structural steel. Part 5 - Technical delivery conditions for structural steels with improved atmospheric corrosion resistance

European steel grades designation systems. New standard EN 10025-5 : 2004 are similar but not identical to EN 10155:1993. Standard EN 10025:2004 published in six parts, here you can find steel grades and numbers for EN 10025-5:2004 - Part 5 standard:

Steel grade
Number
   
   
   


Symbols used in EN 10025 - 5 : 2004 . Structural steel with improved atmospheric corrosion resistance: 

S... - Structural steel; 

.355... - Minimum yield strength (Reh) in MPa at to 16mm; 

...J0.. - Longitudinal Charpy V-notch impacts 27 J at 0°C ; 

...J2.. - Longitudinal Charpy V-notch impacts 27 J at - 20°C; 

....W - Improved atmospheric corrosion resistance; 

....P - Greater phosphorus content (grade 355 only); 

...K2.. - Longitudinal Charpy V-notch impacts 40 J at - 20°C; 

...+AR - Supply in as rolled conditions ; 

...+N - Supply in normalized/normalized rolled condition.

Back